Concentration: | 5% | Clean Temp: | 30 To 80degree |
---|---|---|---|
Type Of Clean: | Soak And DC Current | Clean Time: | 0.5~2 Mins |
Cleaning Objects: | Blind Hole/Dead End/putty/carbon Deposit | Diluted: | 1:20(1kg Powder Diluted 20L Water) |
Density Current: | 1-8A/dm2 |
Product Feature
1. Cathode, anode electrically release oil
2. Good Wash ability, low foam
3. Can suppress the generation of alkali mist
4. Increase the cleanliness and hydrophilicity of the workpiece surface, improve the bonding force between the body and the coating.
Diluted
1:20, 5% concentration, (1kg powder diluted with 20L water )
Package
25Kg/Bag, 2 years warranty, Stock avoid light, Keep cool and dry, air tight .
Delivery time & shipping
Samples 1 day
Large production for 3 days
Shipping: By air /By sea
Common problem & Solve
1 | Products lumps |
products stock not in sealed |
2 | Not clean |
increasing temperature, delay cleaning time change the place of the work pieces. Increase the frequency of ultrasonic equipment. |
3 | solutons getting Black |
circulation filtering , change solution |
4 |
Product discoloration |
The temperature exceeds the range, there is relatively inactive metal ion pollution, remove the source of pollution. |
5 |
Workpiece dissolution |
The work piece is connected to positive conductance, and the work piece needs to be connected to negative electricity |
6 |
High foam |
current density is too big , low down the current and increase the temperature |
Noted
1,Long-term exposure will cause lumps,Unopened but there are remaining products should be sealed and stored, so as not to affect the use effect |
2,Not suitable for Alu product, Or they will bubble reaction. |
3.Normally use Cathode electric release oil, The anode is electrically relieved of oil, which is easy to damage the workpiece |
4.Can use for copper, brass etc product release oil. But can not finished cleaning copper then cleaning the iron steel. Avoid iron steel discoloration. |
Application
Stainless steel product and normal steel iron product , plastic degrease.
Contact Person: Mr. David
Tel: 13682556146
Fax: 86-0755-84804963
25L IT industry Circuit board solder paste spray cleaning fluid
Lemon odour heavy stains remover Range hood Kitchen Essential product
24Kt Without Cyanide Brush Gold Plating Solution Pocerlain Copper Plating Fluids
Cyanide free brighter gold plating solution speical for nickle material
Speical for Stainless Steel Surface Treatment Water Base Rust Inhibitor Solutions
Iron Ware Surface Green Anti Rust Solution Is Most Suitable For Replace Anti Rust Oil